In contrast hydrometallurgical methods are reasonable from an economic point of view. In the following section, ... However, this feature provides vast opportunities for developing new, selective and refined methods of vanadium extraction. Contrarily, the design of organic compounds with lower toxicity and fewer costs, mainly amines, for ...Web
The traditional roasting technique using sodium salts in vanadium production has been disadvantageous due to the large consumption of energy and the emission of harmful gases. A modified process using molten salt roasting and water leaching to extract vanadium and titanium from domestic titanomagnetite concentrate was …Web
The excessive input of heavy metals such as vanadium (V) into the environment has been one of the consequences of global industrial development. Excessive exposure to V can pose a potential threat to …Web
Therefore, establishing a scientific, reasonable, and convenient assessment method for CP is the primary problem to the process of vanadium extraction from stone coal. In light of the complicated nonlinear CP assessment system, characteristics such as small sample sizes and complexity should be considered when choosing the method.Web
Vanadium plays an important role as an alloying element in several types of steel. ... Production capacity will be mothballed to keep prices at a reasonable . ... an extract from "Illusions of ...Web
metalloporphyrins; Yuan et al. [8] considered vanadium extraction techniques from all ... allization residues in reasonable detail. The recovery of metals from spent catalysts andWeb
Li et al. studied vanadium extraction of vS coming from Panzhihua Steel & Iron (Group) Corporation, the oxidation process of vanadium in vS was enhanced in the …Web
The conventional V2O5 preparation processes include ion exchange, chemical precipitation, solvent extraction, and other processes. Given the long process and complex operation nature of traditional V2O5 …Web
An innovative and sustainable way for production of vanadium is to co-process vanadium titanomagnetite ores with vanadium-bearing slag from steel industry, via reduction, producing a hot metal containing about 2 mass% vanadium, 0.1 mass% phosphorus, and 0.4 mass% silicon. A vanadium-extraction method was developed for …Web
High-chromium vanadium residue (HCVR (HCVR: high-chromium vanadium residue)) is an important secondary resource of valuable metals such as vanadium (V), chromium (Cr), and molybdenum (Mo). The mainstream technology for the utilization of HCVR, the Na2CO3-assisted-roasting–water-leaching method, usually requires roasting …Web
This review paper critically examines the compositional differences between steel and petcoke slags and the various extraction methods that apply to vanadium production, particularly from petcoke, …Web
Xiang et al. (2018b) investigated the extraction of vanadium from converter slag by two-step sulfuric acid leaching after calcification roasting. In the first leaching stage, about 81.8% of vanadium was dissolved at a pH of 2.5 in solution, and in the second leaching stage, 8.1% of vanadium was dissolved at pH 0.Web
VO 2+ ions are strongly complexed by porphyrins and related chelators, and the enrichment of crude oil with vanadium is due to its extraction from vanadium-bearing rock by porphyrins present in oil that had passed through rocky layers. Natural release of vanadium mainly goes back to weathering of vanadium-containing rock and the erosion …Web
Boiler ash, or oil ash, is a solid waste produced by burning heavy fuel oil (HFO) in electrical power plants. In addition to carbon, it usually contains V (4.4–19.2%) and Ni (2.7–8.5%), and therefore, they are regarded as promising resources for vanadium extraction [1,2,3].More than 4000 metric tons of oil ashes are generated annually from …Web
The analysis shows that the loss of the organic phase, steps of extraction and stripping of vanadium, extensive extraction and separation times, and occurrence …Web
The typical process route roasting-leaching-precipitation is the most widely used process because of its low cost, simplicity of operation, scalability and high vanadium extraction efficiency. Some reviews on vanadium extraction from stone coal and VTM have been published (Gilligan and Nikoloski, 2020, Lee et al., 2021, Taylor et al., 2006 ...Web
The extraction of high-purity metallic vanadium usually includes two steps: the producing of crude metallic vanadium and the refining of crude metallic vanadium. …Web
In this study, a clean pellet production method of calcium roasting and sulfuric acid leaching of vanadium from vanadium and titanium magnetite concentrates is proposed, which can effectively separate vanadium and iron, and the pellets after acid leaching and vanadium extraction can be used as raw material for iron making after …Web
The results illustrated that the vanadium extraction with different extraction temperatures all increased continuously when the extraction time raised from 1 min to 3 min. ... vanadium anion should contain 3 moles of negative charge. Based on the above analysis, it was considered that the most reasonable anion form of vanadium (V) might …Web
From this concentrate the radium may be extracted and refined by any suitable method. By the procedure outlined, it is possible to get a radium concentrate carrying 50 to 100 milligrams of radium per ton of concentrate, the exact proportion depending on the grade of the ore treated. PART 1: Radium, Uranium & Vanadium …Web
It can be seen from Figure Figure1 1 that the pH value and the extractants have significant effects on the extraction efficiency of vanadium. The extractants of P507 and Cyanex272 reached maximum vanadium extraction efficiencies of 72 and 64% respectively, at a pH value of 1.5, while a maximum vanadium extraction efficiency of …Web
Black shale ore contains rich strategic metal resources such as vanadium, nickel, and molybdenum, but due to its complex composition, it is currently only used in the vanadium extraction industry. Metals such as nickel and molybdenum have not been effectively recovered, resulting in environmental pollution and resource waste. Using …Web
Abstract Vanadium extraction process demands low residual vanadium and carbon loss, and variations of dissolved elements in hot metal must be determined to achieve it. A three parts dynamic model …Web
During the vanadium extraction process in basic oxygen furnace (BOF), unduly high temperature is unfavorable to achieve efficient vanadium yield with minimum carbon loss. A new temperature strategy was developed based on industrial experiments. The new strategy applies the selective oxidation temperature between carbon and …Web
Vanadium(V) oxide as a Catalyst. During the Contact Process for manufacturing sulfuric acid, sulfur dioxide has to be converted into sulfur xide, which is done by passing sulfur dioxide and oxygen …Web
The similar composition of petcoke and steel slags and the forms in which vanadium is present in them make steel slags a reasonable analog to petcoke with regards to vanadium extraction. This is especially important due to the limited literature available on vanadium extraction from petcoke, while vanadium extraction from steel slags is ...Web
According to Fig. 1, a reasonable set of MnO content measured by m(MnO)/m(V 2 O 3) in vanadium slag can be determined as 0.50, 0.65, 0.80, 1.00, 1.35 …Web
The vanadium extraction for above traditional process is about 80% and less than of 5% of chromium is also extracted simultaneously (Liu et al., 2013, Zheng et al., 2012). The high chromium content in the leaching residue posed a big environmental problem unsolved so far in China. In addition, the vanadium extraction is far from satisfied.Web
Deng et al. researched vanadium extraction using Na 2 CO 3 and MnO 2 as additives for vS roasted at 600℃ for 120 min, ... WLR still has value for recycling extraction, on the other hand, the WLR may pose a threat to the environment without reasonable treatment. The WLR is usually transported to the tailings pond for storage, and part of …Web
Extraction procedure Preparation of pregnant solution. The workable sulfate leach liquor for V, Ni, and Zn extraction was made by combining 645 g of the magnetic fraction concentrate from boiler fly ash with 180 g/L H 2 SO 4 under optimal agitation leaching conditions. The final volume of the produced sulfate leach liquid (after filtering …Web